Welding Processes and Joint Design

Manufacturing & Additive ManufacturingPrimary ProcessesđŸŸĸ Free Lesson

Welding Processes and Joint Design

What You'll Learn

  • 1Match SMAW, GMAW, FCAW, GTAW, and SAW to their applications
  • 2Compute arc heat input from voltage, current, efficiency, and travel speed
  • 3Size a fillet weld from throat area and allowable throat stress
  • 4Apply carbon equivalent rules to preheat decisions

A joint that passes visual inspection can still fail at half the design load because the groove was too narrow for root fusion or heat input burned the grain structure. Welding design is a chain: process sets penetration, penetration sets the groove, groove sets deposition volume, and deposition sets distortion. This lesson covers the five arc processes, the heat input equation with its efficiency factors, joint geometry with throat arithmetic, and the carbon equivalent rule that decides preheat.

Theory and Foundations

An arc weld converts electrical energy to heat at the arc, forms a molten pool, and the pool solidifies as the arc moves away. Three quantities must be controlled: energy delivered per unit length, the joint geometry that receives it, and the cooling rate that follows. The assumptions are a quasi-stationary arc, heat losses lumped into one arc efficiency, and weld metal matching the filler classification.

Heat input is the governing energy statement: arc power is voltage times current, divided by travel speed after efficiency is applied:

where is the arc efficiency, is arc voltage in volts, is current in amperes, is travel speed in millimeters per second, and comes out in joules per millimeter. When speed is quoted in millimeters per minute, the conversion is

with in millimeters per minute. Efficiency varies: about 0.40 for gas tungsten arc welding, 0.80 for gas metal arc, 0.85 for shielded metal arc, and 0.90 to 0.95 for submerged arc under its flux blanket.

Low heat input cools fast and can harden a low-alloy heat-affected zone to martensite, while high heat input coarsens prior austenite grains and lowers toughness. That is why every procedure carries a heat input range, not a single number.

Joint geometry follows thickness and access: a square groove suits plate up to about 6 mm, a single V from 6 to 20 mm, a double V or double bevel above 12 mm to halve deposited volume, and a U groove above 40 mm where beveling a wide V wastes more metal than it saves. The deposited cross-section of a single V groove with included angle on thickness is approximately

which shows why halving the groove angle on a thick joint removes a large fraction of the filler and with it the distortion filler volume drives.

Fillet welds are sized on their throat, not on their leg. For an equal-leg fillet of leg size the throat is

and the throat area of length is . The weld carries load in shear on that throat:

and the design check compares that stress with the allowable throat stress, which AWS D1.1 takes as 0.30 times the filler tensile strength:

where is 480 MPa for an E70XX consumable, giving an allowable of 145 MPa on the throat.

Preheat is decided by chemistry. AWS D1.1 computes a carbon equivalent from the specified composition,

and then reads minimum preheat from CE together with joint thickness. Working rule: CE below 0.40 needs no preheat up to 25 mm, CE 0.40 to 0.50 needs about 100 degrees Celsius above 13 mm, and CE above 0.50 needs 150 degrees Celsius at any thickness. Preheat slows cooling, lets hydrogen diffuse out before the martensite start range, and reduces the restrained contraction stress that causes hydrogen cracking.

Key Formulas

The allowable strength check completes the set: a single fillet pass per unit length resists

so for an E70XX bead of 6 mm leg the capacity is N per millimeter, which the designer multiplies by weld length for joint capacity.

Worked Examples

ProcessCurrent rangeTypical fillerArc efficiencyBest use
SMAWAC or DC, 50 to 200 AE7018, E60100.85Field, out-of-position
GMAWDC, 150 to 300 AER70S-60.80Sheet, thin plate
FCAWDC, 200 to 400 AE71T-10.85Thick plate, high rate
GTAWDCEN, 40 to 150 AER308L0.40Root passes, stainless
SAWDCEP, 600 to 1,500 AF7A20.95Long seams, heavy plate

Real-World Examples

  • Structural beam - A 20 mm flange is welded with E7018 low-hydrogen stick at 120 A after preheating to 100 degrees Celsius because the carbon equivalent sits near 0.46.
  • Pipeline seam - A 14 mm line pipe girth weld uses a GMAW root pass and FCAW cap, with peak heat input held below 1.0 kJ/mm to keep the toughness of the coarse-grained zone.
  • Pressure vessel shell - A 30 mm shell seam is submerged arc welded at 1,000 A in a double-V groove, which halves deposition against a single V of the same thickness.
  • Stainless pipe - A 316L tube is GTAW welded with ER308L filler and 99.99 percent argon backing at 90 A, accepting the low efficiency because the root must be fully fused and free of oxide.

💡Set the Root Opening First

Fix root opening and land on the drawing before anything else, because they control fusion and distortion more than any other joint dimension, and every other groove angle is dimensioned from them.

Common Mistakes

Choosing a double-V groove out of habit

Fix: Use a single V under 12 mm and a double V above it, since groove area grows with the square of thickness.

Welding high-carbon steel with no preheat

Fix: Compute carbon equivalent first and preheat above about 0.50 CE regardless of thickness.

Treating heat input as a fixed machine setting

Fix: Recompute it whenever voltage, current, or travel speed changes, since speed is the least stable.

Key Takeaways

  • Heat input is eta times V times I divided by speed, in joules per millimeter
  • Fillet strength is checked on the throat, where a equals 0.707 times the leg
  • Allowable throat stress is 0.30 times filler tensile strength, 145 MPa for E70
  • Carbon equivalent sets preheat, and CE above 0.50 means 150 degrees Celsius

Frequently Asked Questions

What is the difference between SMAW and FCAW?

SMAW uses a flux-coated stick that must be replaced as it burns, while FCAW feeds tubular wire continuously at a higher deposition rate, which is why FCAW dominates thick plate in a shop and SMAW dominates field work.

Why does heat input need an efficiency factor?

No arc converts all its electrical energy into the workpiece. Efficiency runs from about 0.40 for gas tungsten welding, where heat radiates from the pointed arc, to 0.95 for submerged arc under its insulating flux blanket.

When is a backing strip required?

When a groove is welded from one side only and full penetration is required, because the strip supports the molten root. Without it the root must be ground out and backgouged before the second side is welded.

Interview Questions

Q1: How do you prevent cracking in a high-strength steel weld?

Control hydrogen with low-hydrogen filler stored dry, preheat from carbon equivalent, and stay inside the procedure heat input range.

Q2: How do you choose between a V and a U groove?

Below 40 mm a V is cheaper to machine; above it the U groove removes less metal per joint and the bevel cost repays itself.

CW

ChatWhole Learn Editorial Team

Written by experienced data scientists, software engineers, and educators. All content is reviewed by industry professionals to ensure accuracy and relevance.

Last reviewed: 2026-09-27

—
☆☆☆☆☆
0 ratings

Rate & Feedback

Related Tutorials

Content with similar topics across other courses

Continue Learning

Suggested next tutorials based on this topic

Need Expert Manufacturing & Additive Manufacturing Help?

Get personalized tutoring, project support, or professional consulting.

Advertisement